Corrosion of metals and alloys - Stress corrosion cracking - Part 11 : guidelines for testing the resistance of metals and alloys to hydrogen embrittlement and hydrogen-assisted cracking

ISO 7539-11:2013 gives guidance on the key features that should be accounted for in designing and conducting tests to evaluate the resistance of a metal or its alloy to hydrogen embrittlement and hydrogen-assisted cracking.

View the extract
Main informations

Collections

International ISO standards

Publication date

April 2013

Number of pages

16 p.

Reference

ISO 7539-11:2013

ICS Codes

77.060   Corrosion of metals

Print number

1
Sumary
Corrosion of metals and alloys - Stress corrosion cracking - Part 11 : guidelines for testing the resistance of metals and alloys to hydrogen embrittlement and hydrogen-assisted cracking

ISO 7539-11:2013 gives guidance on the key features that should be accounted for in designing and conducting tests to evaluate the resistance of a metal or its alloy to hydrogen embrittlement and hydrogen-assisted cracking.

ZOOM ON ... the Requirements department
To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:
- mandatory clauses to satisfy,
- non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document “ISO / IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents ”as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!

With Requirements, quickly access the main part of the normative text!
Need to identify, monitor and decipher standards?

COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.

Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!

Request your free, no-obligation live demo

I discover COBAZ