NF EN ISO 15609-5
Specification and qualification of welding procedures for metallic materials - Welding procedure specification - Part 5 : resistance welding
ISO 15609-5:2011 specifies requirements for the content of welding procedure specifications for resistance spot, seam, butt and projection welding processes. It is necessary to establish the acceptability of applying the principles of ISO 15609-5:2011 to other resistance and related welding processes before any qualification is undertaken. Variables listed in ISO 15609-5:2011 are those influencing either weld dimensions (quality), weld nugget dimension, weld pattern positioning, mechanical properties or geometry of the welded joint.
ISO 15609-5:2011 specifies requirements for the content of welding procedure specifications for resistance spot, seam, butt and projection welding processes. It is necessary to establish the acceptability of applying the principles of ISO 15609-5:2011 to other resistance and related welding processes before any qualification is undertaken.
Variables listed in ISO 15609-5:2011 are those influencing either weld dimensions (quality), weld nugget dimension, weld pattern positioning, mechanical properties or geometry of the welded joint.
Le présent document spécifie les exigences relatives au contenu des descriptifs de modes opératoires de soudage pour les procédés de soudage par résistance par points, à la molette, en bout et par bossages.
- Avant-proposiv
-
1 Domaine d'application1
-
2 Références normatives1
-
3 Termes et définitions2
-
4 Contenu technique d'un descriptif de mode opératoire de soudage2
-
4.1 Généralités2
-
4.2 Fabricant du produit2
-
4.3 Matériaux de base2
-
4.4 Commun à tous les modes opératoires de soudage3
- Annexe A (informative) Exemple de DMOS - I: Exigences prévues pour les procédés6
- Annexe B (informative) Exemple de DMOS . Il: Critères d'acceptation de la qualité7
- Annexe C (informative) Exemple de DMOS . IlI: Réglage de la machine de soudage8
- Annexe D (informative) Exemples de paramètres de soudage par résistance9
- Bibliographie14
The Requirements department helps you quickly locate within the normative text:
- mandatory clauses to satisfy,
- non-essential but useful clauses to know, such as permissions and recommendations.
The identification of these types of clauses is based on the document “ISO / IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents ”as well as on a constantly enriched list of verbal forms.
With Requirements, quickly access the main part of the normative text!
COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.
Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!
Request your free, no-obligation live demo
I discover COBAZ