NF EN ISO 15613

NF EN ISO 15613

October 2004
Standard Current

Specification and qualification of welding procedures for metallic materials - Qualification based on pre-production welding test

ISO 15613:2004 specifies how a preliminary welding procedure specification is qualified based on pre-production welding tests. It is applicable to arc welding, gas welding, beam welding, resistance welding, stud welding and friction welding of metallic materials. The use of ISO 15613:2004 can be restricted by an application standard or specification.

View the extract
Main informations

Collections

National standards and national normative documents

Publication date

October 2004

Number of pages

12 p.

Reference

NF EN ISO 15613

ICS Codes

25.160.10   Welding processes

Classification index

A89-056

Print number

1 - 23/09/2004

International kinship

European kinship

EN ISO 15613:2004
Sumary
Specification and qualification of welding procedures for metallic materials - Qualification based on pre-production welding test

ISO 15613:2004 specifies how a preliminary welding procedure specification is qualified based on pre-production welding tests.

It is applicable to arc welding, gas welding, beam welding, resistance welding, stud welding and friction welding of metallic materials.

The use of ISO 15613:2004 can be restricted by an application standard or specification.

Replaced standards (1)
NF EN 288-8
July 1995
Standard Cancelled
Specification and approval of welding procedures for metallic mateirals. Part 8 : approval by a pre-production welding test.

Le présent document spécifie les conditions de qualification d'un mode opératoire de soudage par exécution d'assemblages soudés particuliers préalables à la production et précise le domaine d'application ainsi que les limites de validité.

Table of contents
View the extract
  • Avant-propos
    3
  • Introduction
    4
  • 1 Domaine d'application
    4
  • 2 Références normatives
    4
  • 3 Termes et définitions
    5
  • 4 Descriptif du mode opératoire de soudage préliminaire (DMOS-P)
    6
  • 5 Qualification du mode opératoire de soudage
    6
  • 6 Soudage des assemblages de qualification
    6
  • 7 Contrôle, examen et essai
    6
  • 7.1 Soudage par fusion
    6
  • 7.2 Soudage par résistance
    6
  • 8 Domaine de validité
    7
  • 8.1 Généralités
    7
  • 9 Durée de validité
    7
  • 10 Procès-verbal de qualification de mode opératoire de soudage (PV-QMOS)
    7
  • Annexe ZA (informative) Relation entre la présente norme européenne et les exigences essentielles de la Directive UE
    8
ZOOM ON ... the Requirements department
To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:
- mandatory clauses to satisfy,
- non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document “ISO / IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents ”as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!

With Requirements, quickly access the main part of the normative text!
Need to identify, monitor and decipher standards?

COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.

Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!

Request your free, no-obligation live demo

I discover COBAZ