NF EN ISO 15613
Specification and qualification of welding procedures for metallic materials - Qualification based on pre-production welding test
ISO 15613:2004 specifies how a preliminary welding procedure specification is qualified based on pre-production welding tests. It is applicable to arc welding, gas welding, beam welding, resistance welding, stud welding and friction welding of metallic materials. The use of ISO 15613:2004 can be restricted by an application standard or specification.
ISO 15613:2004 specifies how a preliminary welding procedure specification is qualified based on pre-production welding tests.
It is applicable to arc welding, gas welding, beam welding, resistance welding, stud welding and friction welding of metallic materials.
The use of ISO 15613:2004 can be restricted by an application standard or specification.
Le présent document spécifie les conditions de qualification d'un mode opératoire de soudage par exécution d'assemblages soudés particuliers préalables à la production et précise le domaine d'application ainsi que les limites de validité.
- Avant-propos3
- Introduction4
-
1 Domaine d'application4
-
2 Références normatives4
-
3 Termes et définitions5
-
4 Descriptif du mode opératoire de soudage préliminaire (DMOS-P)6
-
5 Qualification du mode opératoire de soudage6
-
6 Soudage des assemblages de qualification6
-
7 Contrôle, examen et essai6
-
7.1 Soudage par fusion6
-
7.2 Soudage par résistance6
-
8 Domaine de validité7
-
8.1 Généralités7
-
9 Durée de validité7
-
10 Procès-verbal de qualification de mode opératoire de soudage (PV-QMOS)7
- Annexe ZA (informative) Relation entre la présente norme européenne et les exigences essentielles de la Directive UE8
The Requirements department helps you quickly locate within the normative text:
- mandatory clauses to satisfy,
- non-essential but useful clauses to know, such as permissions and recommendations.
The identification of these types of clauses is based on the document “ISO / IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents ”as well as on a constantly enriched list of verbal forms.
With Requirements, quickly access the main part of the normative text!
COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.
Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!
Request your free, no-obligation live demo
I discover COBAZ