Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 12 : spot, seam and projection welding

ISO 15614-12:2004 specifies the tests which may be used for qualification of welding procedure specifications for spot, seam and projection welding processes. ISO 15614-12:2004 defines the conditions for carrying out tests and the limits of validity of a qualified welding procedure for all practical welding operations covered by this International Standard. Tests shall be carried out in accordance with this International Standard unless more severe tests are specified by the relevant application standard or contract when these shall apply. The acceptability of applying the principles of this International Standard to other resistance welding processes should be established before any qualification is undertaken. ISO 15614-12:2004 covers the following resistance welding processes: - spot welding; - indirect spot welding; - direct spot welding; - seam welding; - lap seam welding; - mash seam welding; - fail butt-seam welding; - seam welding with strip; - projection welding; - indirect projection welding; - direct projection welding.

View the extract
Main informations

Collections

National standards and national normative documents

Publication date

December 2004

Number of pages

16 p.

Reference

NF EN ISO 15614-12

ICS Codes

25.160.10   Welding processes

Classification index

A89-057-12

Print number

1 - 18/11/2004

International kinship

European kinship

EN ISO 15614-12:2004
Sumary
Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 12 : spot, seam and projection welding

ISO 15614-12:2004 specifies the tests which may be used for qualification of welding procedure specifications for spot, seam and projection welding processes.

ISO 15614-12:2004 defines the conditions for carrying out tests and the limits of validity of a qualified welding procedure for all practical welding operations covered by this International Standard.

Tests shall be carried out in accordance with this International Standard unless more severe tests are specified by the relevant application standard or contract when these shall apply.

The acceptability of applying the principles of this International Standard to other resistance welding processes should be established before any qualification is undertaken.

ISO 15614-12:2004 covers the following resistance welding processes:

- spot welding;

- indirect spot welding;

- direct spot welding;

- seam welding;

- lap seam welding;

- mash seam welding;

- fail butt-seam welding;

- seam welding with strip;

- projection welding;

- indirect projection welding;

- direct projection welding.

Standard replaced by (1)
NF EN ISO 15614-12
September 2014
Standard Cancelled
Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 12 : spot, seam and projection welding

<p>ISO 15614-12:2014 specifies the tests which can be used for qualification of welding procedure specifications for spot, seam, and projection welding processes. It is part of the ISO 15614 series, details of which are given in ISO 15607, Annex A. ISO 15614-12:2014 defines the conditions for carrying out tests and the limits of validity of a qualified welding procedure for all practical welding operations covered by it.</p>

Table of contents
View the extract
  • Avant-propos
    3
  • Introduction
    4
  • 1 Domaine d'application
    4
  • 2 Références normatives
    5
  • 3 Termes et définitions
    5
  • 4 Descriptif de mode opératoire de soudage préliminaire (DMOS-P)
    5
  • 5 Épreuve de qualification de mode opératoire de soudage
    6
  • 6 Assemblage de qualification
    6
  • 6.1 Généralités
    6
  • 6.2 Formes et dimensions des assemblages de qualification et des éprouvettes pour les essais destructifs
    6
  • 6.3 Soudage des composants, des assemblages de qualification et des éprouvettes
    6
  • 7 Contrôles, examens et essais
    7
  • 7.1 Étendue des contrôles, examens et essais
    7
  • 7.2 Positions et prélèvement des éprouvettes
    9
  • 7.3 Essais non destructifs
    9
  • 7.4 Contre-essais
    9
  • 8 Domaine de validité
    9
  • 8.1 Généralités
    9
  • 8.2 Par rapport au fabricant
    9
  • 8.3 Par rapport au matériau
    9
  • 8.4 Commun à tous les modes opératoires de soudage
    10
  • 9 Procès-verbal de qualification de mode opératoire de soudage (PV-QMOS)
    10
Need to identify, monitor and decipher standards?

COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.

Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!

Request your free, no-obligation live demo

I discover COBAZ