NF EN ISO 15614-13
Specification and qualificationl of welding procedures for metallic materials - Welding procedure test - Part 13 : resistance butt and flash welding
ISO 15614-13:2005 specifies the tests which should be used for qualification of welding procedure specifications. It applies to resistance butt welding and flash welding of metallic materials, e.g. with solid, tubular, flat or circular cross-section. The basic principles of ISO 15614-13:2005 may be applied to other resistance welding processes when this is specified in the specification. ISO 15614-13:2005 defines the conditions for carrying out tests and the limits of validity of a qualified welding procedure for all practical welding operations covered by ISO 15614-13:2005. ISO 15614-13:2005 covers the following resistance welding processes as defined in ISO 4063: 24 flash welding using direct current or alternating current with various movement sequences, constant flashing and pulsed flashing; 25 resistance butt welding, using direct current or alternating current with various pressure sequences.
ISO 15614-13:2005 specifies the tests which should be used for qualification of welding procedure specifications.
It applies to resistance butt welding and flash welding of metallic materials, e.g. with solid, tubular, flat or circular cross-section. The basic principles of ISO 15614-13:2005 may be applied to other resistance welding processes when this is specified in the specification.
ISO 15614-13:2005 defines the conditions for carrying out tests and the limits of validity of a qualified welding procedure for all practical welding operations covered by ISO 15614-13:2005.
ISO 15614-13:2005 covers the following resistance welding processes as defined in ISO 4063:
24 flash welding using direct current or alternating current with various movement sequences, constant flashing and pulsed flashing;
25 resistance butt welding, using direct current or alternating current with various pressure sequences.
<p>ISO 15614-13:2012 specifies tests for the qualification of welding procedure specifications applicable to upset (resistance butt) welding and flash welding of metallic materials, e.g. with solid, tubular, flat or circular cross-section. Its basic principles can also be applied to other resistance welding processes when this is stated in the specification.</p> <p>ISO 15614-13:2012 defines the conditions for carrying out tests and the limits of validity of a qualified welding procedure for all the practical welding operations that it covers. The tests required to qualify the procedure for a particular component or assembly depend on the performance and quality requirements of the component or assembly, as defined in the design specification. The tests are intended to be carried out in accordance with the requirements of ISO 15614-13:2012, unless more severe tests are specified by the relevant application standard or specification and when these apply.</p> <p>ISO 15614-13:2012 covers the following resistance welding processes, as defined in ISO 4063: 24 flash welding, using direct current or alternating current with various movement sequences, constant flashing and pulsed flashing; 25 resistance upset welding, using direct current or alternating current with various pressure sequences.</p>
- Avant-proposiv
- Introductionvi
-
1Domaine d'application 1
-
2Références normatives 2
-
3Termes et définitions 3
-
4Descriptif de mode opératoire de soudage préliminaire (DMOS-P) 3
-
5Épreuve de qualification du mode opératoire de soudage 3
-
6Assemblage de qualification et éprouvette 4
-
6.1 Généralités4
-
6.2Forme et dimensions des éprouvettes 4
-
6.3Soudage des composants, des assemblages de qualification ou des éprouvettes 6
-
7Essais et contrôle 6
-
7.1Étendue du contrôle 6
-
7.2Essais non destructifs 6
-
7.3Essais destructifs 7
-
7.4Coupe macrographique 7
-
7.5Filiation de dureté 7
-
7.6Contre-essais 7
-
8Domaine de validité 8
-
8.1 Généralités8
-
8.2 Fabricant8
-
8.3Métaux de base 8
-
8.4Modes opératoires de soudage 8
-
8.5Certificat de qualification 8
-
9Procès-verbal de qualification du mode opératoire de soudage (PV-QMOS) 8
- Annexe A (informative) Exemple de qualification de mode opératoire de soudage - Certificat de qualification9
- Annexe B (informative) Exemple de procès-verbal de qualification de mode opératoire de
- soudage (PV-QMOS)11
The Requirements department helps you quickly locate within the normative text:
- mandatory clauses to satisfy,
- non-essential but useful clauses to know, such as permissions and recommendations.
The identification of these types of clauses is based on the document “ISO / IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents ”as well as on a constantly enriched list of verbal forms.
With Requirements, quickly access the main part of the normative text!
COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.
Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!
Request your free, no-obligation live demo
I discover COBAZ