Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 8 : welding of tubes to tube-plate joints

This European Standard specifies requirements for the qualification testing of welding procedures for the arc welding of tube to tube-plate joints in metallic materials by manual, partly mechanized, mechanized or automatic processes. This standard is a part of a series of standards. Details of this series are given in prEN ISO 15607, Annex A. Qualification by tube to tube-plate joint tests can be used for all joints even if they are fully loaded or only seal welded as required in application standards. In such cases, one or more special test pieces should be made to simulate the production joint in all essential features, e.g. dimensions, restraint, heat sink effects. The test should be carried out prior to and under the conditions to be used in production. This standard applies to fusion welding of metallic materials for tube to tube-plate joints with gap. This standard does not apply to tube-sheets with forged end connections with welded tubes (external/internal bore welds). For welding of tube to tube-plate joints without gap welding procedure test should be defined in the specification. For other applications and/or requirements the standard can be used if required by the specification. Repair welding should be considered in the welding procedure test.

View the extract
Main informations

Collections

National standards and national normative documents

Publication date

July 2002

Number of pages

27 p.

Reference

NF EN ISO 15614-8

ICS Codes

25.160.10   Welding processes

Classification index

A89-057-8

Print number

1 - 07/12/2002

International kinship

European kinship

EN ISO 15614-8:2002
Sumary
Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 8 : welding of tubes to tube-plate joints

This European Standard specifies requirements for the qualification testing of welding procedures for the arc welding of tube to tube-plate joints in metallic materials by manual, partly mechanized, mechanized or automatic processes.

This standard is a part of a series of standards. Details of this series are given in prEN ISO 15607, Annex A. Qualification by tube to tube-plate joint tests can be used for all joints even if they are fully loaded or only seal welded as required in application standards.

In such cases, one or more special test pieces should be made to simulate the production joint in all essential features, e.g. dimensions, restraint, heat sink effects. The test should be carried out prior to and under the conditions to be used in production.

This standard applies to fusion welding of metallic materials for tube to tube-plate joints with gap. This standard does not apply to tube-sheets with forged end connections with welded tubes (external/internal bore welds). For welding of tube to tube-plate joints without gap welding procedure test should be defined in the specification.

For other applications and/or requirements the standard can be used if required by the specification.

Repair welding should be considered in the welding procedure test.

Standard replaced by (1)
NF EN ISO 15614-8
September 2016
Standard Current
Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 8 : welding of tubes to tube-plate joints

<p>ISO 15614-8:2016 specifies requirements for the qualification testing of welding procedures for the arc welding of tube to tube-plate joints in metallic materials by manual, partly mechanized, fully mechanized, or automatic processes.</p> <p>ISO 15614-8:2016 is a part of a series of standards. Details of this series are given in ISO 15607, Annex A.</p> <p>Qualification by tube to tube-plate joint tests can be used for all joints even if they are fully loaded or only seal welded as required in application standards.</p> <p>ISO 15614-8:2016 applies to fusion welding of metallic materials for tube to tube-plate joints with a remaining gap between the tube and the tube-plate for some length of the tube-plate thickness. This part of ISO 15614 does not apply to tube-sheets with forged end connections with welded tubes (external/internal bore welds).</p> <p>For welding of tube to tube-plate joints with mechanical expansion which is load bearing, welding procedure test is to be defined.</p> <p>For other applications and/or requirements, this part of ISO 15614 can be used if required by the specification.</p> <p>Repair welding is to be considered in the welding procedure test.</p>

Table of contents
View the extract
  • Avant-propos
    3
  • 1 Domaine d'application
    4
  • 2 Références normatives
    4
  • 3 Termes, définitions et symboles
    5
  • 3.1 Termes et définitions
    5
  • 3.2 Symboles
    5
  • 4 Descriptif d'un mode opératoire de soudage préliminaire (DMOS-P)
    6
  • 4.1 Généralités
    6
  • 4.2 Informations concernant tous les procédés de soudage
    6
  • 4.3 Informations concernant des procédés de soudage particuliers
    7
  • 5 Qualification du mode opératoire de soudage
    7
  • 6 Soudage des assemblages de qualification
    8
  • 6.1 Généralités
    8
  • 6.2 Type de l'assemblage de qualification
    8
  • 7 Examens, contrôles et essais
    9
  • 7.1 Exécution
    9
  • 7.2 Critères d'acceptation
    11
  • 8 Domaine de validité
    13
  • 8.1 Généralités
    13
  • 8.2 Par rapport au constructeur
    13
  • 8.3 Par rapport au matériau
    14
  • 8.4 Dispositions communes à tous les modes opératoires de soudage
    14
  • 9 Procès-verbal de qualification de mode opératoire de soudage (PV-QMOS)
    16
  • Annexe A (informative) Procès-verbal de qualification de mode opératoire de soudage de tubes sur plaque tubulaire (PV-QMOS)
    17
  • Annexe ZA (informative) Articles de la présente norme européenne concernant les exigences essentielles ou d'autres dispositions des Directives UE
    22
  • Bibliographie
    23
Need to identify, monitor and decipher standards?

COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.

Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!

Request your free, no-obligation live demo

I discover COBAZ