NF EN ISO 7539-6

NF EN ISO 7539-6

June 2003
Standard Cancelled

Corrosion of metals and alloys - Stress corrosion testing - Part 6 : preparation and use of pre-cracked specimens for tests under constant load or constant displacement

ISO 7539-6:2002 covers procedures for designing, preparing and using pre-cracked specimens for investigating susceptibility to stress corrosion. It gives recommendations for the design, preparation and use of pre-cracked specimens for investigating susceptibility to stress corrosion. The term "metal" as used in this part of ISO 7539 includes alloys. Because of the need to confine plasticity at the crack tip, pre-cracked specimens are not suitable for the evaluation of thin products such as sheet or wire and are generally used for thicker products including plate bar and forgings. They can also be used for parts joined by welding.

View the extract
Main informations

Collections

National standards and national normative documents

Publication date

June 2003

Number of pages

47 p.

Reference

NF EN ISO 7539-6

ICS Codes

77.060   Corrosion of metals

Classification index

A05-501-6

Print number

1 - 18/06/2003

International kinship

ISO 7539-6:2003

European kinship

EN ISO 7539-6:2003
Sumary
Corrosion of metals and alloys - Stress corrosion testing - Part 6 : preparation and use of pre-cracked specimens for tests under constant load or constant displacement

ISO 7539-6:2002 covers procedures for designing, preparing and using pre-cracked specimens for investigating susceptibility to stress corrosion. It gives recommendations for the design, preparation and use of pre-cracked specimens for investigating susceptibility to stress corrosion.

The term "metal" as used in this part of ISO 7539 includes alloys.

Because of the need to confine plasticity at the crack tip, pre-cracked specimens are not suitable for the evaluation of thin products such as sheet or wire and are generally used for thicker products including plate bar and forgings. They can also be used for parts joined by welding.

Replaced standards (1)
NF EN ISO 7539-6
October 1995
Standard Cancelled
Corrosion of metals and alloys. Stress corrosion testing. Part 6 : preparation and use of pre-cracked specimens.

Standard replaced by (1)
NF EN ISO 7539-6
December 2011
Standard Cancelled
Corrosion of metals and alloys - Stress corrosion testing - Part 6 : preparation and use of precracked specimens for tests under constant load or constant displacement

<p>ISO 7539-6:2011 covers procedures for designing, preparing and using precracked specimens for investigating susceptibility to stress corrosion. It gives recommendations for the design, preparation and use of precracked specimens for investigating susceptibility to stress corrosion. </p> <p>The term "metal" as used in ISO 7539-6:2011 includes alloys.</p> <p>Because of the need to confine plasticity at the crack tip, precracked specimens are not suitable for the evaluation of thin products, such as sheet or wire, and are generally used for thicker products including plate bar and forgings. They can also be used for parts joined by welding.</p> <p>Precracked specimens can be loaded with equipment for application of a constant load or can incorporate a device to produce a constant displacement at the loading points. Tests conducted under increasing displacement or increasing load are dealt with in ISO 7539-9.</p> <p>A particular advantage of precracked specimens is that they allow data to be acquired from which critical defect sizes, above which stress corrosion cracking can occur, can be estimated for components of known geometry subjected to known stresses. They also enable rates of stress corrosion crack propagation to be determined. The latter data can be taken into account when monitoring parts containing defects during service.</p>

Table of contents
View the extract
  • Avant-propos
    iv
  • 1 Domaine d'application
    1
  • 2
    Références normatives 1
  • 3
    Termes et définitions 2
  • 4
    Principe 4
  • 5
    Éprouvettes 5
  • 6
    Amorçage et propagation de la fissure de fatigue 24
  • 7
    Mode opératoire 26
  • 8
    Rapport d'essai 34
  • Annexe A (normative) Utilisation d'éprouvettes entaillées pour essais de corrosion sous contrainte
    36
  • Annexe B (normative) Détermination de la vitesse de propagation de la fissuration
    39
Need to identify, monitor and decipher standards?

COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.

Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!

Request your free, no-obligation live demo

I discover COBAZ