NF EN ISO 7539-6
Corrosion of metals and alloys. Stress corrosion testing. Part 6 : preparation and use of pre-cracked specimens.
<p>ISO 7539-6:2002 covers procedures for designing, preparing and using pre-cracked specimens for investigating susceptibility to stress corrosion. It gives recommendations for the design, preparation and use of pre-cracked specimens for investigating susceptibility to stress corrosion.</p> <p>The term "metal" as used in this part of ISO 7539 includes alloys.</p> <p>Because of the need to confine plasticity at the crack tip, pre-cracked specimens are not suitable for the evaluation of thin products such as sheet or wire and are generally used for thicker products including plate bar and forgings. They can also be used for parts joined by welding.</p>
COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.
Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!
Request your free, no-obligation live demo
I discover COBAZ