ASTM A1001-18

septembre 2018
Norme En vigueur

Standard Specification for High-Strength Steel Castings in Heavy Sections

This specification covers cast alloy steels in the normalized and tempered or quenched and tempered condition, suitable for high strain gradient conditions. One test block for each heat is required. The test block configuration and size are specified. Tension and Charpy impact tests and oxygen, nitrogen, and hydrogen gas content tests shall be performed. The steel shall be made by electric furnace process with methods, such as argon-oxygen-decarburization, to conform to the maximum gas level. Heat treatment procedure shall be done. Multiple austenitizing and tempering are permitted. The chemistry grade shall conform to the required chemical composition for carbon, manganese, phosphorus, sulfur, silicon, nickel, chromium, molybdenum, and aluminum. Residual elements include: zirconium, copper, titanium, tungsten, vanadium, columbium, and boron. A product analysis shall be made for specification conformance. Casting shell and core depth zone shall be established and examined. Repair methods such as grinding and welding are detailed.

Information importante
Pour la consultation de ce document, l'installation du plug in FileOpen est nécessaire.
la consultation du document est disponible uniquement en version PDF avec une utilisation monoposte et l'impression n'est pas autorisée.
Si ce n'est pas déjà fait, téléchargez le plug-in ICI
Consultez ICI nos prérequis.
Informations générales

Collections

Normes américaines ASTM

Date de publication

septembre 2018

Nombre de pages

6 p.

Référence

ASTM A1001-18

Indice de classement

A1001-18
Résumé
Standard Specification for High-Strength Steel Castings in Heavy Sections

This specification covers cast alloy steels in the normalized and tempered or quenched and tempered condition, suitable for high strain gradient conditions. One test block for each heat is required. The test block configuration and size are specified. Tension and Charpy impact tests and oxygen, nitrogen, and hydrogen gas content tests shall be performed. The steel shall be made by electric furnace process with methods, such as argon-oxygen-decarburization, to conform to the maximum gas level. Heat treatment procedure shall be done. Multiple austenitizing and tempering are permitted. The chemistry grade shall conform to the required chemical composition for carbon, manganese, phosphorus, sulfur, silicon, nickel, chromium, molybdenum, and aluminum. Residual elements include: zirconium, copper, titanium, tungsten, vanadium, columbium, and boron. A product analysis shall be made for specification conformance. Casting shell and core depth zone shall be established and examined. Repair methods such as grinding and welding are detailed.

Qu'est-ce que le format Redline ?
Le service Redline+ - comparateur de normes vous permet d’identifier facilement et simplement les changements majeurs entre la norme en vigueur et sa dernière version annulée.

D’un simple coup d’oeil, vous pourrez identifier les ajouts, suppressions ou modifications à un texte, tableau, figure et formule.
D’un simple coup d’oeil, vous pourrez identifier les ajouts, suppressions ou modifications à un texte, tableau, figure et formule

Le service Redlines+ vous est proposé sur la collection des normes françaises en vigueur, en langue Française et au format HTML et PDF.

Pour un aperçu du service, veuillez cliquer sur Visualiser une norme au format redline
Besoin d’identifier, de veiller et de décrypter les normes ?

COBAZ est la solution simple et efficace pour répondre aux besoins normatifs liés à votre activité, en France comme à l’étranger.

Disponible sur abonnement, CObaz est LA solution modulaire à composer selon vos besoins d’aujourd’hui et de demain. Découvrez vite CObaz !

Demandez votre démo live gratuite, sans engagement

Je découvre COBAZ