A la demande de l’éditeur, la consultation du document est disponible uniquement en version PDF avec une utilisation monoposte et l'impression n'est pas autorisée. Si vous n’êtes pas la personne destinée à utiliser ce document, ne pas le télécharger sur votre poste, sinon cette dernière ne pourra pas l’ouvrir.
ASTM A703/A703M-20a
Standard Specification for Steel Castings, General Requirements, for Pressure-Containing Parts
This specification covers steel castings, general requirements, for pressure-containing parts. The steel shall be made by open-hearth or electric-furnace process, with or without separate refining such as argon-oxygen-decarburization (AOD), unless otherwise designated by the individual specification. Ferritic and martensitic steel shall be cooled after pouring to provide substantially complete transformation of austenite prior to heat treatment to enhance mechanical properties. The material shall conform to the specified chemical composition requirements. An analysis of each heat shall be made by the manufacturer to determine the percentages of the elements specified. The mechanical test methods and definitions are presented in details. One tension test shall be made from each heat, and shall conform to the tensile requirements specified. Test coupons shall be cast from the same heat as the castings represented, except that for investment castings, the test coupons shall be cast in the same type of mold as the castings. After machining, each casting shall be tested under specified hydrostatic shell test pressures in the applicable steel rating for which the casting is designed.
A la demande de l’éditeur, la consultation du document est disponible uniquement en version PDF avec une utilisation monoposte et l'impression n'est pas autorisée. Si vous n’êtes pas la personne destinée à utiliser ce document, ne pas le télécharger sur votre poste, sinon cette dernière ne pourra pas l’ouvrir.
Collections
Date de publication
Nombre de pages
Référence
Indice de classement
This specification covers steel castings, general requirements, for pressure-containing parts. The steel shall be made by open-hearth or electric-furnace process, with or without separate refining such as argon-oxygen-decarburization (AOD), unless otherwise designated by the individual specification. Ferritic and martensitic steel shall be cooled after pouring to provide substantially complete transformation of austenite prior to heat treatment to enhance mechanical properties. The material shall conform to the specified chemical composition requirements. An analysis of each heat shall be made by the manufacturer to determine the percentages of the elements specified. The mechanical test methods and definitions are presented in details. One tension test shall be made from each heat, and shall conform to the tensile requirements specified. Test coupons shall be cast from the same heat as the castings represented, except that for investment castings, the test coupons shall be cast in the same type of mold as the castings. After machining, each casting shall be tested under specified hydrostatic shell test pressures in the applicable steel rating for which the casting is designed.
This specification covers steel castings, general requirements, for pressure-containing parts. The steel shall be made by open-hearth or electric-furnace process, with or without separate refining such as argon-oxygen-decarburization (AOD), unless otherwise designated by the individual specification. Ferritic and martensitic steel shall be cooled after pouring to provide substantially complete transformation of austenite prior to heat treatment to enhance mechanical properties. The material shall conform to the specified chemical composition requirements. An analysis of each heat shall be made by the manufacturer to determine the percentages of the elements specified. The mechanical test methods and definitions are presented in details. One tension test shall be made from each heat, and shall conform to the tensile requirements specified. Test coupons shall be cast from the same heat as the castings represented, except that for investment castings, the test coupons shall be cast in the same type of mold as the castings. After machining, each casting shall be tested under specified hydrostatic shell test pressures in the applicable steel rating for which the casting is designed.
D’un simple coup d’oeil, vous pourrez identifier les ajouts, suppressions ou modifications à un texte, tableau, figure et formule.

Le service Redlines+ vous est proposé sur la collection des normes françaises en vigueur, en langue Française et au format HTML et PDF.
Pour un aperçu du service, veuillez cliquer sur Visualiser une norme au format redline
COBAZ est la solution simple et efficace pour répondre aux besoins normatifs liés à votre activité, en France comme à l’étranger.
Disponible sur abonnement, CObaz est LA solution modulaire à composer selon vos besoins d’aujourd’hui et de demain. Découvrez vite CObaz !
Demandez votre démo live gratuite, sans engagement
Je découvre COBAZ