NF EN ISO 7539-10
Corrosion of metals and alloys - Stress corrosion testing - Part 10 : reverse U-bend method
This document specifies procedures for designing, preparing and using reversed U-bend (RUB) test specimens for investigating the susceptibility of the metal to stress corrosion cracking. The term "metal" as used in this document includes alloys.
This document specifies procedures for designing, preparing and using reversed U-bend (RUB) test specimens for investigating the susceptibility of the metal to stress corrosion cracking. The term "metal" as used in this document includes alloys.
<p>ISO 7539-10:2013 covers procedures for designing, preparing and using reversed U-bend (RUB) test specimens for investigating the susceptibility of the metal to stress corrosion cracking. The term "metal" as used in this standard includes alloys.</p>
- Avant-propos
-
1 Domaine d'application
-
2 Références normatives
-
3 Termes et définitions
-
4 Principe
-
5 Éprouvettes
-
6 Mode opératoire expérimental
-
7 Évaluation après exposition
-
8 Rapport d'essai
- Annexe A (informative) Préparation d'éprouvettes RUB en demi-tube non prédéformées
- Annexe B (informative) Préparation d'éprouvettes RUB à section calibrée
- Bibliographie
The Requirements department helps you quickly locate within the normative text:
- mandatory clauses to satisfy,
- non-essential but useful clauses to know, such as permissions and recommendations.
The identification of these types of clauses is based on the document “ISO / IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents ”as well as on a constantly enriched list of verbal forms.
With Requirements, quickly access the main part of the normative text!
At a glance, you will be able to identify the additions, deletions or modifications to a text, table, figure and formula.
The Redlines + service is offered to you on the collection of French standards in force, in French language and in HTML and PDF format.
For an overview of the service, click on View a standard in redline format
COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.
Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!
Request your free, no-obligation live demo
I discover COBAZ