NF EN ISO 7539-10
Corrosion of metals and alloys - Stress corrosion testing - Part 10 : reverse U-bend method
ISO 7539-10:2013 covers procedures for designing, preparing and using reversed U-bend (RUB) test specimens for investigating the susceptibility of the metal to stress corrosion cracking. The term "metal" as used in this standard includes alloys.
ISO 7539-10:2013 covers procedures for designing, preparing and using reversed U-bend (RUB) test specimens for investigating the susceptibility of the metal to stress corrosion cracking. The term "metal" as used in this standard includes alloys.
<p>This document specifies procedures for designing, preparing and using reversed U-bend (RUB) test specimens for investigating the susceptibility of the metal to stress corrosion cracking. The term "metal" as used in this document includes alloys.</p>
- Avant-propos
-
1 Domaine d'application
-
2 Référence normative
-
3 Termes et définitions
-
4 Principe
-
5 Éprouvettes
-
6 Mode opératoire expérimental
-
7 Évaluation après exposition
-
8 Rapport d'essai
- Annexe A (informative) Préparation d'une éprouvette RUB en demi-tube non prédéformée
- Annexe B (informative) Éprouvettes RUB à section calibrée
COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.
Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!
Request your free, no-obligation live demo
I discover COBAZ