DIN EN ISO 11357-2

DIN EN ISO 11357-2

August 2020
Standard Current

Plastics - Differential scanning calorimetry (DSC) - Part 2: Determination of glass transition temperature and step height (ISO 11357-2:2020) - German version EN ISO 11357-2:2020

Main informations

Collections

DIN german standards

Publication date

August 2020

Number of pages

17 p.

Reference

DIN EN ISO 11357-2

ICS Codes

83.080.01   Plastics in general

Print number

1
Replaced standards (1)
DIN EN ISO 11357-2
July 2014
Standard Cancelled
Plastics - Differential scanning calorimetry (DSC) - Part 2: Determination of glass transition temperature and glass transition step height (ISO 11357-2:2013), German version EN ISO 11357-2:2014

Need to identify, monitor and decipher standards?

COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.

Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!

Request your free, no-obligation live demo

I discover COBAZ