Plastics - Differential scanning calorimetry (DSC) - Part 1: General principles

The ISO 11357 series specifies several differential scanning calorimetry (DSC) methods for the thermal analysis of polymers and polymer blends, such as—    thermoplastics (polymers, moulding compounds and other moulding materials, with or without fillers, fibres or reinforcements),—    thermosets (uncured or cured materials, with or without fillers, fibres or reinforcements), and—    elastomers (with or without fillers, fibres or reinforcements).The ISO 11357 series is applicable for the observation and measurement of various properties of, and phenomena associated with, the above-mentioned materials, such as—    physical transitions (glass transition, phase transitions such as melting and crystallization, polymorphic transitions, etc.),—    chemical reactions (polymerization, crosslinking and curing of elastomers and thermosets, etc.),—    the stability to oxidation, and—    the heat capacity.This document specifies a number of general aspects of differential scanning calorimetry, such as the principle and the apparatus, sampling, calibration and general aspects of the procedure and test report common to all parts.Details on performing specific methods are given in subsequent parts of the ISO 11357 series (see Foreword).

View the extract
Main informations

Collections

International ISO standards

Publication date

February 2023

Number of pages

34 p.

Reference

ISO 11357-1:2023

ICS Codes

83.080.01   Plastics in general

Print number

1
Sumary
Plastics - Differential scanning calorimetry (DSC) - Part 1: General principles

The ISO 11357 series specifies several differential scanning calorimetry (DSC) methods for the thermal analysis of polymers and polymer blends, such as

—    thermoplastics (polymers, moulding compounds and other moulding materials, with or without fillers, fibres or reinforcements),

—    thermosets (uncured or cured materials, with or without fillers, fibres or reinforcements), and

—    elastomers (with or without fillers, fibres or reinforcements).

The ISO 11357 series is applicable for the observation and measurement of various properties of, and phenomena associated with, the above-mentioned materials, such as

—    physical transitions (glass transition, phase transitions such as melting and crystallization, polymorphic transitions, etc.),

—    chemical reactions (polymerization, crosslinking and curing of elastomers and thermosets, etc.),

—    the stability to oxidation, and

—    the heat capacity.

This document specifies a number of general aspects of differential scanning calorimetry, such as the principle and the apparatus, sampling, calibration and general aspects of the procedure and test report common to all parts.

Details on performing specific methods are given in subsequent parts of the ISO 11357 series (see Foreword).

Replaced standards (1)
ISO 11357-1:2016
ISO 11357-1:2016
September 2016
International standard Cancelled
Plastics - Differential scanning calorimetry (DSC) - Part 1: General principles

ISO 11357-1:2016 specifies several differential scanning calorimetry (DSC) methods for the thermal analysis of polymers and polymer blends, such as - thermoplastics (polymers, moulding compounds and other moulding materials, with or without fillers, fibres or reinforcements), - thermosets (uncured or cured materials, with or without fillers, fibres or reinforcements), and - elastomers (with or without fillers, fibres or reinforcements). ISO 11357-1:2016 is intended for the observation and measurement of various properties of, and phenomena associated with, the above-mentioned materials, such as - physical transitions (glass transition, phase transitions such as melting and crystallization, polymorphic transitions, etc.), - chemical reactions (polymerization, crosslinking and curing of elastomers and thermosets, etc.), - the stability to oxidation, and - the heat capacity. ISO 11357-1:2016 specifies a number of general aspects of differential scanning calorimetry, such as the principle and the apparatus, sampling, calibration and general aspects of the procedure and test report common to all following parts. Details on performing specific methods are given in subsequent parts of ISO 11357 (see Foreword).

ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


Need to identify, monitor and decipher standards?