ISO 11357-2:2020
ISO 11357-2:2020

ISO 11357-2:2020

March 2020
International standard Current

Plastics - Differential scanning calorimetry (DSC) - Part 2: Determination of glass transition temperature and step height

This document specifies methods for the determination of the glass transition temperature and the step height related to the glass transition of amorphous and partially crystalline plastics.

View the extract
Main informations

Collections

International ISO standards

Publication date

March 2020

Number of pages

9 p.

Reference

ISO 11357-2:2020

ICS Codes

83.080.01   Plastics in general

Print number

1
Sumary
Plastics - Differential scanning calorimetry (DSC) - Part 2: Determination of glass transition temperature and step height

This document specifies methods for the determination of the glass transition temperature and the step height related to the glass transition of amorphous and partially crystalline plastics.

Replaced standards (1)
ISO 11357-2:2013
ISO 11357-2:2013
May 2013
International standard Cancelled
Plastics - Differential scanning calorimetry (DSC) - Part 2 : determination of glass transition temperature and glass transition step height

ISO 11357-2:2013 specifies methods for the determination of the glass transition temperature and the step height related to the glass transition of amorphous and partially crystalline plastics.

ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


What is the Redline format?
Need to identify, monitor and decipher standards?