ISO 11357-7:2022
ISO 11357-7:2022

ISO 11357-7:2022

March 2022
International standard Current

Plastics - Differential scanning calorimetry (DSC) - Part 7: Determination of crystallization kinetics

This document specifies two methods (isothermal and non-isothermal) for studying the crystallization kinetics of partially crystalline polymers using differential scanning calorimetry (DSC).It is only applicable to molten polymers.NOTE       These methods are not suitable if the molecular structure of the polymer is modified during the test.

View the extract
Main informations

Collections

International ISO standards

Publication date

March 2022

Number of pages

13 p.

Reference

ISO 11357-7:2022

ICS Codes

83.080.01   Plastics in general

Print number

1
Sumary
Plastics - Differential scanning calorimetry (DSC) - Part 7: Determination of crystallization kinetics

This document specifies two methods (isothermal and non-isothermal) for studying the crystallization kinetics of partially crystalline polymers using differential scanning calorimetry (DSC).

It is only applicable to molten polymers.

NOTE       These methods are not suitable if the molecular structure of the polymer is modified during the test.

Replaced standards (1)
ISO 11357-7:2015
ISO 11357-7:2015
August 2015
International standard Cancelled
Plastics - Differential scanning calorimetry (DSC) - Part 7 : determination of crystallization kinetics

ISO 11357-7:2015 specifies two methods (isothermal and non-isothermal) for studying the crystallization kinetics of partially crystalline polymers using differential scanning calorimetry (DSC). It is only applicable to molten polymers. NOTE These methods are not suitable if the molecular structure of the polymer is modified during the test.

ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


What is the Redline format?
Need to identify, monitor and decipher standards?