Specification and qualification of welding procedures for production welding of steel and nickel-base castings

This document specifies how a welding procedure specification (WPS) for production welding of steel castings is qualified. Tests are intended to be carried out in accordance with this document, unless additional tests are specified by the purchaser or by agreement between the contracting parties.This document defines the conditions for the execution of welding procedure qualification tests and the limits of validity of a qualified welding procedure for all practical welding operations within the range of essential variables.This document applies to the arc welding of steel castings. The principles of this document can be applied to other fusion welding processes subject to agreement between the contracting parties.

View the extract
Main informations

Collections

International ISO standards

Publication date

November 2025

Number of pages

17 p.

Reference

ISO 11970:2025

ICS Codes

77.140.80   Iron and steel castings
25.160.10   Welding processes

Print number

1
Sumary
Specification and qualification of welding procedures for production welding of steel and nickel-base castings

This document specifies how a welding procedure specification (WPS) for production welding of steel castings is qualified. Tests are intended to be carried out in accordance with this document, unless additional tests are specified by the purchaser or by agreement between the contracting parties.

This document defines the conditions for the execution of welding procedure qualification tests and the limits of validity of a qualified welding procedure for all practical welding operations within the range of essential variables.

This document applies to the arc welding of steel castings. The principles of this document can be applied to other fusion welding processes subject to agreement between the contracting parties.

Replaced standards (1)
ISO 11970:2016
ISO 11970:2016
March 2016
International standard Cancelled
Specification and qualification of welding procedures for production welding of steel castings

ISO 11970:2016 specifies how a welding procedure specification (WPS) for production welding of steel castings is qualified. It defines the conditions for the execution of welding procedure qualification tests and the limits of validity of a qualified welding procedure for all practical welding operations within the range of essential variables. Tests are intended to be carried out in accordance with this International Standard unless additional tests are specified by the purchaser or by agreement between the contracting parties. ISO 11970:2016 applies to the arc welding of steel castings. The principles of this International Standard can be applied to other fusion welding processes subject to agreement between the contracting parties. In the case of specific service, material or manufacturing conditions, tests more comprehensive than those specified by this International Standard can be specified by the purchaser, in order to gain more information, e.g. longitudinal weld tensile tests, bend tests, chemical analyses, ferrite determination in austenitic stainless steels, elongation, Charpy "V" impact tests, and radiography.

ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


What is the Redline format?
Need to identify, monitor and decipher standards?