ISO 15607:2019
ISO 15607:2019

ISO 15607:2019

October 2019
International standard Current

Specification and qualification of welding procedures for metallic materials - General rules

This document is part of a series of standards dealing with specification and qualification of welding procedures. Annex A gives details of this series of standards, Annex B gives a table for the use of these standards, and Annex C gives a flow diagram for the development and qualification of a WPS.This document defines general rules for the specification and qualification of welding procedures for metallic materials. This document also refers to several other standards as regards detailed rules for specific applications.This document is applicable to manual, partly mechanized, fully mechanized and automated welding.Welding procedures are qualified by conforming to one or more welding procedure qualification records (WPQR). The use of a particular method of qualification is often a requirement of an application standard.It is assumed that welding procedure specifications are used in production by competent welders, qualified in accordance with the relevant part of ISO 9606 or by competent operators qualified in accordance with ISO 14732.

View the extract
Main informations

Collections

International ISO standards

Publication date

October 2019

Number of pages

10 p.

Reference

ISO 15607:2019

ICS Codes

25.160.10   Welding processes

Print number

1
Sumary
Specification and qualification of welding procedures for metallic materials - General rules

This document is part of a series of standards dealing with specification and qualification of welding procedures. Annex A gives details of this series of standards, Annex B gives a table for the use of these standards, and Annex C gives a flow diagram for the development and qualification of a WPS.

This document defines general rules for the specification and qualification of welding procedures for metallic materials. This document also refers to several other standards as regards detailed rules for specific applications.

This document is applicable to manual, partly mechanized, fully mechanized and automated welding.

Welding procedures are qualified by conforming to one or more welding procedure qualification records (WPQR). The use of a particular method of qualification is often a requirement of an application standard.

It is assumed that welding procedure specifications are used in production by competent welders, qualified in accordance with the relevant part of ISO 9606 or by competent operators qualified in accordance with ISO 14732.

Replaced standards (2)
ISO 15607:2003
ISO 15607:2003
December 2003
International standard Cancelled
Specification and qualification of welding procedures for metallic materials - General rules

ISO 15607:2003 defines general rules for the specification and qualification of welding procedures for metallic materials. It also refers to several other standards as regards detailed rules for specific applications. ISO 15607:2003 is applicable to manual, mechanized and automatic welding.

ISO 15607/AC1:2005
ISO 15607/AC1:2005
September 2005
International standard Cancelled
Technical corrigendum 1 to standard ISO 15607:2003

ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.