Specification and qualification of welding procedures for metallic materials - Welding procedure specification - Part 5 : resistance welding

ISO 15609-5:2011 specifies requirements for the content of welding procedure specifications for resistance spot, seam, butt and projection welding processes. It is necessary to establish the acceptability of applying the principles of ISO 15609-5:2011 to other resistance and related welding processes before any qualification is undertaken.Variables listed in ISO 15609-5:2011 are those influencing either weld dimensions (quality), weld nugget dimension, weld pattern positioning, mechanical properties or geometry of the welded joint.

View the extract
Main informations

Collections

International ISO standards

Publication date

October 2011

Number of pages

13 p.

Reference

ISO 15609-5:2011

ICS Codes

25.160.10   Welding processes

Print number

2 - décembre 2011
Sumary
Specification and qualification of welding procedures for metallic materials - Welding procedure specification - Part 5 : resistance welding

ISO 15609-5:2011 specifies requirements for the content of welding procedure specifications for resistance spot, seam, butt and projection welding processes. It is necessary to establish the acceptability of applying the principles of ISO 15609-5:2011 to other resistance and related welding processes before any qualification is undertaken.

Variables listed in ISO 15609-5:2011 are those influencing either weld dimensions (quality), weld nugget dimension, weld pattern positioning, mechanical properties or geometry of the welded joint.

ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


Need to identify, monitor and decipher standards?