ISO 15611:2024
ISO 15611:2024

ISO 15611:2024

January 2024
International standard Current

Specification and qualification of welding procedures for metallic materials - Qualification based on previous welding experience

This document gives the necessary information to explain the requirements referenced in ISO 15607 about the qualification of welding procedures based on previous welding experience.In addition, it gives the range of qualification.The use of this document can be restricted by an application standard or a specification.

View the extract
Main informations

Collections

International ISO standards

Publication date

January 2024

Number of pages

2 p.

Reference

ISO 15611:2024

ICS Codes

25.160.01   Welding, brazing and soldering in general

Print number

1
Sumary
Specification and qualification of welding procedures for metallic materials - Qualification based on previous welding experience

This document gives the necessary information to explain the requirements referenced in ISO 15607 about the qualification of welding procedures based on previous welding experience.

In addition, it gives the range of qualification.

The use of this document can be restricted by an application standard or a specification.

Replaced standards (1)
ISO 15611:2003
ISO 15611:2003
December 2003
International standard Cancelled
Specification and qualification of welding procedures for metallic materials - Qualification based on previous welding experience

ISO 15611:2003 gives the necessary information to explain the requirements referenced in ISO 15607 concerning the qualification of welding procedures based on previous welding experience. In addition it gives the range of qualification and the validity. The use of ISO 15611:2003 may be restricted by an application standard or a specification.

ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


What is the Redline format?
Need to identify, monitor and decipher standards?