Specification and qualification of welding procedures for metallic materials - Qualification by adoption of a standard welding procedure specification

This document:— specifies how a user can follow a standard welding procedure specification (SWPS) based on welding procedure qualification tests performed by a different organization;— specifies the range for the use of SWPSs in accordance with ISO 15607;— specifies the requirements for qualification of welding procedures to be issued as SWPSs; and— specifies the requirements for organizations adopting SWPSs.The use of this document can be restricted by an application standard or a specification.This document is applicable to welding of steels and aluminium and its alloys (see 4.1).All new standard welding procedure qualifications are to be carried out in accordance with this document from the date of its issue. However, this document does not invalidate previous standard welding procedure qualifications made to former standards, specifications or previous editions of this document

View the extract
Main informations

Collections

International ISO standards

Publication date

June 2018

Number of pages

5 p.

Reference

ISO 15612:2018

ICS Codes

25.160.10   Welding processes

Print number

1
Sumary
Specification and qualification of welding procedures for metallic materials - Qualification by adoption of a standard welding procedure specification

This document:

— specifies how a user can follow a standard welding procedure specification (SWPS) based on welding procedure qualification tests performed by a different organization;

— specifies the range for the use of SWPSs in accordance with ISO 15607;

— specifies the requirements for qualification of welding procedures to be issued as SWPSs; and

— specifies the requirements for organizations adopting SWPSs.

The use of this document can be restricted by an application standard or a specification.

This document is applicable to welding of steels and aluminium and its alloys (see 4.1).

All new standard welding procedure qualifications are to be carried out in accordance with this document from the date of its issue. However, this document does not invalidate previous standard welding procedure qualifications made to former standards, specifications or previous editions of this document

Replaced standards (1)
ISO 15612:2004
ISO 15612:2004
August 2004
International standard Cancelled
Specification and qualification of welding procedures for metallic materials - Qualification by adoption of a standard welding procedure

ISO 15612:2004 gives the information necessary to explain the requirements referenced in ISO 15607 about qualification by adoption of a standard welding procedure, and establishes the conditions, limits and ranges of qualification necessary for the use of a standard welding procedure. This International Standard gives the manufacturer the possibility of using welding procedures based on welding procedure tests performed by other organisations. The use of ISO 15612:2004 can be restricted by an application standard or a specification.

ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


What is the Redline format?
Need to identify, monitor and decipher standards?