ISO 15614-12:2021
Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 12: Spot, seam and projection welding
This document specifies the tests which can be used for qualification of welding procedure specifications for spot, seam, and projection welding processes.NOTE The procedures are written for embossed projection welding. They can be adapted for solid projections as well, e.g. nut welding, stud welding. cross wire welding.This document defines the conditions for carrying out tests and the limits of validity of a qualified welding procedure for all practical welding operations covered by this document.It covers the following resistance welding processes, as defined in ISO 4063:— 21 – resistance spot welding;— 211 – indirect spot welding;— 212 – direct spot welding;— 22 – resistance seam welding;— 221 – lap seam welding;— 222 – mash seam welding;— 223 – Prep-lap seam welding;— 224 – Wire seam welding;— 225 – foil butt-seam welding;— 226 – seam welding with strip;— 23 – projection welding;— 231 – indirect projection welding;— 232 – direct projection welding.
This document specifies the tests which can be used for qualification of welding procedure specifications for spot, seam, and projection welding processes.
NOTE The procedures are written for embossed projection welding. They can be adapted for solid projections as well, e.g. nut welding, stud welding. cross wire welding.
This document defines the conditions for carrying out tests and the limits of validity of a qualified welding procedure for all practical welding operations covered by this document.
It covers the following resistance welding processes, as defined in ISO 4063:
— 21 – resistance spot welding;
— 211 – indirect spot welding;
— 212 – direct spot welding;
— 22 – resistance seam welding;
— 221 – lap seam welding;
— 222 – mash seam welding;
— 223 – Prep-lap seam welding;
— 224 – Wire seam welding;
— 225 – foil butt-seam welding;
— 226 – seam welding with strip;
— 23 – projection welding;
— 231 – indirect projection welding;
— 232 – direct projection welding.
ISO 15614-12:2014 specifies the tests which can be used for qualification of welding procedure specifications for spot, seam, and projection welding processes. It is part of the ISO 15614 series, details of which are given in ISO 15607, Annex A. ISO 15614-12:2014 defines the conditions for carrying out tests and the limits of validity of a qualified welding procedure for all practical welding operations covered by it.
To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.
The Requirements department helps you quickly locate within the normative text:
- mandatory clauses to satisfy,
- non-essential but useful clauses to know, such as permissions and recommendations.
The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.
With Requirements, quickly access the main part of the normative text!

At a glance, you will be able to identify the additions, deletions or modifications to a text, table, figure and formula.

The Redlines + service is offered to you on the collection of French standards in force, in French language and in HTML and PDF format.
For an overview of the service, click on View a standard in redline format
COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.
Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!
Request your free, no-obligation live demo
I discover COBAZ