ISO 15614-2:2025
Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 2: Arc welding of aluminium and its alloys
This document specifies how a preliminary welding procedure specification (pWPS) is qualified by welding procedure tests.This document applies to production welding, repair welding and build-up welding.This document defines the conditions for the execution of welding procedure tests and the range of qualification for welding procedures for all practical welding operations within the qualification of this document.This document applies to the arc welding of wrought and cast aluminium and its alloys. In this document the term aluminium stands for aluminium and for aluminium alloys.This document does not apply to finishing welding of aluminium castings, which is addressed in ISO 15614-4.Arc welding of aluminium is covered by the following welding processes in accordance with ISO 4063:2023:131 ? MIG welding with solid wire electrode;141 ? TIG welding with solid filler material (wire/rod);142 ? Autogenous TIG welding;15 ? plasma arc welding.
This document specifies how a preliminary welding procedure specification (pWPS) is qualified by welding procedure tests.
This document applies to production welding, repair welding and build-up welding.
This document defines the conditions for the execution of welding procedure tests and the range of qualification for welding procedures for all practical welding operations within the qualification of this document.
This document applies to the arc welding of wrought and cast aluminium and its alloys. In this document the term aluminium stands for aluminium and for aluminium alloys.
This document does not apply to finishing welding of aluminium castings, which is addressed in ISO 15614-4.
Arc welding of aluminium is covered by the following welding processes in accordance with ISO 4063:2023:
131 ? MIG welding with solid wire electrode;
141 ? TIG welding with solid filler material (wire/rod);
142 ? Autogenous TIG welding;
15 ? plasma arc welding.
ISO 15614-2:2005 specifies how a preliminary welding procedure specification is qualified by welding procedure tests. It applies to the arc welding of wrought and cast aluminium and its alloys. It does not apply to finishing welding of aluminium castings, which is dealt with by ISO 15614-4.
The Requirements department helps you quickly locate within the normative text:
- mandatory clauses to satisfy,
- non-essential but useful clauses to know, such as permissions and recommendations.
The identification of these types of clauses is based on the document “ISO / IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents ”as well as on a constantly enriched list of verbal forms.
With Requirements, quickly access the main part of the normative text!

COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.
Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!
Request your free, no-obligation live demo
I discover COBAZ