ISO 16433:2006

ISO 16433:2006

April 2006
International standard Current

Resistance welding - Procedure for seam welding of coated and uncoated low carbon steels

ISO16433:2006 specifies requirements for resistance seam welding in the fabrication of assemblies of uncoated and metallic coated low carbon steel comprising two sheets of metal, where the maximum single sheet thickness of components to be welded is within the range 0,4 mm to 3 mm for the following materials:uncoated steels;hot-dip zinc or iron-zinc alloy (galvannealed) coated steel;electrolytic zinc, zinc-iron, or zinc-nickel coated steel;aluminium coated steel;zinc-aluminium coated steel.

View the extract
Main informations

Collections

International ISO standards

Publication date

April 2006

Number of pages

20 p.

Reference

ISO 16433:2006

ICS Codes

25.160.10   Welding processes

Print number

1 - 24/04/2006
Sumary
Resistance welding - Procedure for seam welding of coated and uncoated low carbon steels

ISO16433:2006 specifies requirements for resistance seam welding in the fabrication of assemblies of uncoated and metallic coated low carbon steel comprising two sheets of metal, where the maximum single sheet thickness of components to be welded is within the range 0,4 mm to 3 mm for the following materials:

  • uncoated steels;
  • hot-dip zinc or iron-zinc alloy (galvannealed) coated steel;
  • electrolytic zinc, zinc-iron, or zinc-nickel coated steel;
  • aluminium coated steel;
  • zinc-aluminium coated steel.
ZOOM ON ... the Requirements department
To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:
- mandatory clauses to satisfy,
- non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document “ISO / IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents ”as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!

With Requirements, quickly access the main part of the normative text!
Need to identify, monitor and decipher standards?

COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.

Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!

Request your free, no-obligation live demo

I discover COBAZ