ISO 204:2023

ISO 204:2023

July 2023
International standard Current

Metallic materials - Uniaxial creep testing in tension - Method of test

This document specifies the methods for:a)    uninterrupted creep tests with continuous monitoring of extension;b)    interrupted creep tests with periodic measurement of elongation;c)    stress rupture tests where normally only the time to fracture is measured;d)    a test to verify that a predetermined time can be exceeded under a given force, with the elongation or extension not necessarily being reported.NOTE       A creep test can be continued until fracture has occurred or it can be stopped before fracture.

View the extract
Main informations

Collections

International ISO standards

Publication date

July 2023

Number of pages

48 p.

Reference

ISO 204:2023

ICS Codes

77.040.10   Mechanical testing of metals

Print number

1
Sumary
Metallic materials - Uniaxial creep testing in tension - Method of test

This document specifies the methods for:

a)    uninterrupted creep tests with continuous monitoring of extension;

b)    interrupted creep tests with periodic measurement of elongation;

c)    stress rupture tests where normally only the time to fracture is measured;

d)    a test to verify that a predetermined time can be exceeded under a given force, with the elongation or extension not necessarily being reported.

NOTE       A creep test can be continued until fracture has occurred or it can be stopped before fracture.

Replaced standards (1)
ISO 204:2018
August 2018
International standard Cancelled
Metallic materials - Uniaxial creep testing in tension - Method of test

This document specifies the methods for a) uninterrupted creep tests with continuous monitoring of extension, b) interrupted creep tests with periodic measurement of elongation, c) stress rupture tests where normally only the time to fracture is measured, d) a test to verify that a predetermined time can be exceeded under a given force, with the elongation or extension not necessarily being reported. NOTE A creep test can be continued until fracture has occurred or it can be stopped before fracture.

ZOOM ON ... the Requirements department
To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:
- mandatory clauses to satisfy,
- non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document “ISO / IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents ”as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!

With Requirements, quickly access the main part of the normative text!
Need to identify, monitor and decipher standards?

COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.

Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!

Request your free, no-obligation live demo

I discover COBAZ