ISO 7539-7:2005
ISO 7539-7:2005

ISO 7539-7:2005

February 2005
International standard Current

Corrosion of metals and alloys - Stress corrosion testing - Part 7 : method for slow strain rate testing

ISO 7539-7:2005 covers procedures for conducting slow strain rate tests for investigating susceptibility of a metal to stress corrosion cracking, including hydrogen-induced failure. The term "metal" as used in this part of ISO 7539 includes alloys.Slow strain rate tests are adaptable for testing a wide variety of product forms, including plate, rod, wire, sheet and tubes, as well as composites of these and parts joined by welding. Notched specimens may be used, as well as initially plain specimens.The principal advantage of the test is the rapidity with which susceptibility to stress corrosion cracking of a particular metal/environment combination can be assessed.

View the extract
Main informations

Collections

International ISO standards

Publication date

February 2005

Number of pages

7 p.

Reference

ISO 7539-7:2005

ICS Codes

77.060   Corrosion of metals

Print number

1 - février 2005
Sumary
Corrosion of metals and alloys - Stress corrosion testing - Part 7 : method for slow strain rate testing

ISO 7539-7:2005 covers procedures for conducting slow strain rate tests for investigating susceptibility of a metal to stress corrosion cracking, including hydrogen-induced failure. The term "metal" as used in this part of ISO 7539 includes alloys.

Slow strain rate tests are adaptable for testing a wide variety of product forms, including plate, rod, wire, sheet and tubes, as well as composites of these and parts joined by welding. Notched specimens may be used, as well as initially plain specimens.

The principal advantage of the test is the rapidity with which susceptibility to stress corrosion cracking of a particular metal/environment combination can be assessed.

Replaced standards (1)
ISO 7539-7:1989
ISO 7539-7:1989
December 1989
International standard Cancelled
Corrosion of metals and alloys. Stress corrosion testing. Part 7 : slow strain rate testing.

ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


Need to identify, monitor and decipher standards?