NF EN ISO 11357-3
NF EN ISO 11357-3

NF EN ISO 11357-3

March 2013
Standard Cancelled

Plastics - Differential scanning calorimetry (DSC) - Part 3 : determination of temperature and enthalpy of melting and crystallization

Main informations

Collections

National standards and national normative documents

Publication date

March 2013

Release date

juin 2018

Number of pages

14 p.

Reference

NF EN ISO 11357-3

ICS Codes

83.080.01   Plastics in general

Print number

1 - février 2013

International kinship

ISO 11357-3:2011

European kinship

EN ISO 11357-3:2013
Replaced standards (1)
NF ISO 11357-3
NF ISO 11357-3
November 2011
Standard Cancelled
Plastics - Differential scanning calorimetry (DSC) - Part 3 : determination of temperature and enthalpy of melting and crystallization

ISO 11357-3:2011 specifies a method for the determination of the temperatures and enthalpies of melting and crystallization of crystalline or partially crystalline plastics.

Standard replaced by (1)
NF EN ISO 11357-3
Standard Cancelled
Plastics — Differential scanning calorimetry (DSC) — Part 3: Determination of temperature and enthalpy of melting and crystallization

ZOOM ON ... the Requirements department
To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:
- mandatory clauses to satisfy,
- non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document “ISO / IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents ”as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!

With Requirements, quickly access the main part of the normative text!
New: UPSELL service
Need to identify, monitor and decipher standards?