Corrosion of metals and alloys. Stress corrosion testing. Part 6 : preparation and use of pre-cracked specimens.

Main informations

Collections

National standards and national normative documents

Publication date

October 1995

Number of pages

36 p.

Reference

NF EN ISO 7539-6

ICS Codes

77.060   Corrosion of metals

Classification index

A05-501-6

Print number

1 - 01/09/1995

International kinship

ISO 7539-6:1989

European kinship

EN ISO 7539-6:1995
Standard replaced by (1)
NF EN ISO 7539-6
June 2003
Standard Cancelled
Corrosion of metals and alloys - Stress corrosion testing - Part 6 : preparation and use of pre-cracked specimens for tests under constant load or constant displacement

ISO 7539-6:2002 covers procedures for designing, preparing and using pre-cracked specimens for investigating susceptibility to stress corrosion. It gives recommendations for the design, preparation and use of pre-cracked specimens for investigating susceptibility to stress corrosion. The term "metal" as used in this part of ISO 7539 includes alloys. Because of the need to confine plasticity at the crack tip, pre-cracked specimens are not suitable for the evaluation of thin products such as sheet or wire and are generally used for thicker products including plate bar and forgings. They can also be used for parts joined by welding.

New: UPSELL service
- The UPSELL service allows you to easily update one of your standards.
- With a single click, add a new language, the Requirements or Redline+ service and add one or more additional users.
- Whether you are in the process of acquiring a standard or it is already available in your personal space, the UPSELL service is available at every stage to help you understand it and implement it within your organization.
Need to identify, monitor and decipher standards?

COBAZ is the simple and effective solution to meet the normative needs related to your activity, in France and abroad.

Available by subscription, CObaz is THE modular solution to compose according to your needs today and tomorrow. Quickly discover CObaz!

Request your free, no-obligation live demo

I discover COBAZ