Corrosion of metals and alloys — Stress corrosion testing — Part 6: Preparation and use of precracked specimens for tests under constant load or constant displacement

Le présent document couvre les procédures de conception, de préparation et d''utilisation d''éprouvettes préfissurées servant à évaluer la sensibilité d''un métal à la corrosion sous contrainte.

Main informations

Collections

National standards and national normative documents

Publication date

September 2018

Number of pages

51 p.

Reference

NF EN ISO 7539-6

ICS Codes

77.060   Corrosion of metals

Print number

1

International kinship

European kinship

EN ISO 7539-6:2018
Sumary
Corrosion of metals and alloys — Stress corrosion testing — Part 6: Preparation and use of precracked specimens for tests under constant load or constant displacement

Le présent document couvre les procédures de conception, de préparation et d''utilisation d''éprouvettes préfissurées servant à évaluer la sensibilité d''un métal à la corrosion sous contrainte.
Replaced standards (1)
NF EN ISO 7539-6
NF EN ISO 7539-6
December 2011
Standard Cancelled
Corrosion of metals and alloys -- Stress corrosion testing -- Part 6: Preparation and use of precracked specimens for tests under constant load or constant displacement

Le présent document couvre les procédures de définition, de préparation et d''utilisation d''éprouvettes préfissurées servant à évaluer la sensibilité d''un métal à la corrosion sous contrainte à l''aide d''essais effectués sous charge constante ou sous déplacement constant.

ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


What is the Redline format?
New: UPSELL service
Need to identify, monitor and decipher standards?