Corrosion of metals and alloys - Stress corrosion testing - Part 11 : guidelines for testing the resistance of metals and alloys to hydrogen embrittlement and hydrogen assisted cracking

ISO 7539-11:2013 gives guidance on the key features that should be accounted for in designing and conducting tests to evaluate the resistance of a metal or its alloy to hydrogen embrittlement and hydrogen-assisted cracking.

Main informations

Collections

National standards and national normative documents

Publication date

February 2015

Number of pages

25 p.

Reference

NF EN ISO 7539-11

ICS Codes

77.060   Corrosion of metals

Classification index

A05-501-11

Print number

1

International kinship

ISO 7539-11:2013

European kinship

EN ISO 7539-11:2014
Sumary
Corrosion of metals and alloys - Stress corrosion testing - Part 11 : guidelines for testing the resistance of metals and alloys to hydrogen embrittlement and hydrogen assisted cracking

ISO 7539-11:2013 gives guidance on the key features that should be accounted for in designing and conducting tests to evaluate the resistance of a metal or its alloy to hydrogen embrittlement and hydrogen-assisted cracking.

Table of contents
  • Avant-propos
    iv
  • 1 Domaine d'application
    1
  • 2 Références normatives
    1
  • 3 Facteurs à prendre en considération dans la fragilisation par l'hydrogène et la fissuration assistée sous hydrogène
    1
  • 4 Choix de la méthode d'essai
    3
  • 5 Évaluation après essai
    14
  • Bibliographie
    15
ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


New: UPSELL service
Need to identify, monitor and decipher standards?