NF EN ISO 7539-5
NF EN ISO 7539-5

NF EN ISO 7539-5

September 1995
Standard Current

Corrosion of metals and alloys - Stress corrosion testing - Part 5: Preparation and use of C-ring specimens (ISO 7539-5:1989)

Main informations

Collections

National standards and national normative documents

Publication date

September 1995

Number of pages

15 p.

Reference

NF EN ISO 7539-5

ICS Codes

77.060   Corrosion of metals

Print number

1 - septembre 1995

International kinship

ISO 7539-5:1989

European kinship

EN ISO 7539-5:1995
ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


New: UPSELL service
Need to identify, monitor and decipher standards?