NF EN ISO 11357-5
NF EN ISO 11357-5

NF EN ISO 11357-5

May 2014
Standard Cancelled

Plastics - Differential scanning calorimetry (DSC) - Part 5 : determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion

ISO 11357-5:2013 specifies a method for the determination of reaction temperatures and times, enthalpies of reaction, and degrees of conversion using differential scanning calorimetry (DSC).The method applies to monomers, prepolymers, and polymers in the solid or liquid state. The material can contain fillers and/or initiators in the solid or liquid state.

Main informations

Collections

National standards and national normative documents

Publication date

May 2014

Number of pages

19 p.

Reference

NF EN ISO 11357-5

ICS Codes

83.080.01   Plastics in general

Classification index

T51-507-5

Print number

1

International kinship

ISO 11357-5:2013

European kinship

EN ISO 11357-5:2014
Sumary
Plastics - Differential scanning calorimetry (DSC) - Part 5 : determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion

ISO 11357-5:2013 specifies a method for the determination of reaction temperatures and times, enthalpies of reaction, and degrees of conversion using differential scanning calorimetry (DSC).

The method applies to monomers, prepolymers, and polymers in the solid or liquid state. The material can contain fillers and/or initiators in the solid or liquid state.

Standard replaced by (1)
NF EN ISO 11357-5
Standard Current
Plastics - Differential scanning calorimetry (DSC) - Part 5: Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion

Table of contents
  • Avant-propos
    iv
  • 1 Domaine d'application
    1
  • 2 Références normatives
    1
  • 3 Termes et définitions
    1
  • 4 Principe
    1
  • 5 Appareillage et matériaux
    2
  • 6 Éprouvettes
    2
  • 7 Conditions d'essai et conditionnement des éprouvettes
    2
  • 8 Étalonnage
    2
  • 9 Mode opératoire
    2
  • 10 Détermination des résultats
    4
  • 11 Fidélité
    9
  • 12 Rapport d'essai
    9
  • Bibliographie
    11
ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


New: UPSELL service
Need to identify, monitor and decipher standards?