NF EN ISO 11357-5
NF EN ISO 11357-5

NF EN ISO 11357-5

May 2025
Standard Current

Plastics - Differential scanning calorimetry (DSC) - Part 5: Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion

Main informations

Collections

National standards and national normative documents

Publication date

May 2025

Number of pages

22 p.

Reference

NF EN ISO 11357-5

ICS Codes

83.080.01   Plastics in general

Print number

1

International kinship

ISO 11357-5:2025

European kinship

EN ISO 11357-5:2025
Replaced standards (1)
NF EN ISO 11357-5
Standard Cancelled
Plastics - Differential scanning calorimetry (DSC) - Part 5 : determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion

ISO 11357-5:2013 specifies a method for the determination of reaction temperatures and times, enthalpies of reaction, and degrees of conversion using differential scanning calorimetry (DSC). The method applies to monomers, prepolymers, and polymers in the solid or liquid state. The material can contain fillers and/or initiators in the solid or liquid state.

ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


What is the Redline format?
New: UPSELL service
Need to identify, monitor and decipher standards?