NF EN ISO 11357-7
NF EN ISO 11357-7

NF EN ISO 11357-7

March 2022
Standard Current

Plastics — Differential scanning calorimetry (DSC) — Part 7: Determination of crystallization kinetics

Le présent document spécifie deux méthodes (isotherme et non isotherme) , permettant d''étudier la cinétique de cristallisation de polymères semi-cristallins en utilisant l''analyse calorimétrique différentielle (DSC). Il s''applique uniquement aux polymères fondus.

Main informations

Collections

National standards and national normative documents

Publication date

March 2022

Number of pages

20 p.

Reference

NF EN ISO 11357-7

ICS Codes

83.080.01   Plastics in general

Print number

1

International kinship

European kinship

EN ISO 11357-7:2022
Sumary
Plastics — Differential scanning calorimetry (DSC) — Part 7: Determination of crystallization kinetics

Le présent document spécifie deux méthodes (isotherme et non isotherme) , permettant d''étudier la cinétique de cristallisation de polymères semi-cristallins en utilisant l''analyse calorimétrique différentielle (DSC). Il s''applique uniquement aux polymères fondus.
Replaced standards (1)
NF EN ISO 11357-7
NF EN ISO 11357-7
November 2015
Standard Cancelled
Plastics - Differential scanning calorimetry (DSC) - Part 7: Determination of crystallization kinetics

Le présent document spécifie deux méthodes (isotherme et non isotherme), permettant d''étudier la cinétique de cristallisation de polymères semi-cristallins en utilisant l''analyse calorimétrique différentielle (DSC). Il s''applique uniquement aux polymères fondus.

ZOOM ON ... the Requirements department

To comply with a standard, you need to quickly understand its issues in order to determine its impact on your activity.

The Requirements department helps you quickly locate within the normative text:

  • mandatory clauses to satisfy,
  • non-essential but useful clauses to know, such as permissions and recommendations.

The identification of these types of clauses is based on the document "ISO/IEC Directives, Part 2 - Principles and rules of structure and drafting of ISO documents" as well as on a constantly enriched list of verbal forms.

With Requirements, quickly access the main part of the normative text!


What is the Redline format?
New: UPSELL service
Need to identify, monitor and decipher standards?